voestalpine Inserts for Test Tubes

    testtubes

    designed for pure performance

    Our AM Inserts for Test Tubes have optimized conformal cooling solutions, enabling our customers to run a stable and highly efficient production with a minimized cost per plastic part produced.

    Our inserts reduce the overall cycle time by up to 30% compared to conventionally manufactured drilled cooling channels. Improved part tolerances are also achieved through homogeneous and conformal cooling design, leading to decreased scrap rates.

    Many globally active plastic injection molding companies in various industries have confirmed the premium functionality and profitability of our corrosion-resistant AM Inserts for Test Tubes.

     

    configure & buy
    Customer benefits
    • Improved cycle time up to 30% --> increased productivity
    • Improved part tolerances --> reduced scrap rate
    • High gloss polishability --> state of the art surface quality (similar to 1.2083)
    • Higher wear resistance --> lifetime increase compared to copper beryllium inserts
    • Corrosion resistant material --> improved crack resistance
    Product Features

    Technical Data

    Material premium materials by BÖHLER/Uddeholm
    Hardness Level 49 – 53 HRC
    PVD Coating (optional) voestalpine special coatings
    Cooling voestalpine tailored conformal cooling

    Manufacturing Process

    additive_manufacturing

    Technical Data

    Chemical Analysis

    C Si Mn Cr Ni Mo Al
    0.03 0.30 0.30 12.00 9.20 1.40 1.60