+46-563-170 00
High resistance to pitting, crevice and chloride stress corrosion, high resistance to general corrosion in acids, high corrosion fatigue and erosion corrosion, good weldability, High Pitting Resistance Equivalent Number (>40).
Carbon(C) |
Manganes(Mn) |
Phosphorus(P) |
Sulfur(S) |
Silicon(Si) |
Nickel(Ni) |
Cobalt(Co) |
0.030 Max | 1.2 Max | 0.025 Max | 0.015 Max | 0.8 Max | 6.0-8.0 | – |
Chromium(Cr) |
Manganese(Mo) |
Niobium + Tantalum(Nb (Cb) + Ta) |
Titanium(Ti) |
Copper(Cu) |
Aluminum(Al) |
Iron (Fe) & Others |
24.0-26.0 | 3.0-4.0 | – | – | – | – | PREN– 40 Min, Nitrogen– 0.3, Fe– Balance |