Alloy 625 / UNS N06625 / 2.4856 


Alloy 625 / UNS N06625 / 2.4856 / L625 ENQUIRIES
inconel 718

Alloy 625 / UNS N06625 / 2.4856– High-Strength Corrosion-Resistant Nickel Alloy

Key Features:

  • Excellent resistance to pitting, crevice corrosion, and intergranular attack
  • High strength and toughness across a wide temperature range
  • Good resistance to mineral acids (nitric, phosphoric, sulfuric, hydrochloric)
  • Resistance to alkalis and organic acids
  • Good weldability and formability
  • Chemical processing: reactors, heat exchangers, piping
  • Offshore and marine engineering
  • Environmental technology: flue gas scrubbers, waste incineration
  • Aerospace and power generation
Material number2.4856 
Alloy625
EN designationNiCr22Mo9Nb
UNSN06625
Böhler designationL625
Semi-finished products (strip, sheet, pipe, rod)DIN 17744 / DIN 17752 / DIN EN 10228
Forged or rolled componentsASTM B 446 / ASME SB 446 / ASTM B564 /
DIN 17752/ VdTÜV 499 / AMS 5666
Sheets / strips ASTM B 443 / ASME SB 443 / DIN 17750 /
VdTÜV 499 / AMS 5599
WireDIN 17753 / DIN EN 10088-3 
Pipe / Tube ASTM B 444 / ASME SB 444 / ASTM B 704 / ASME SB 704/ ASTM B 705 / ASME SB 705 / VdTÜV 499
Material Density8.44 g/cm³
Melting Point1290 – 1350°C
Thermal Conductivity (20 °C)9.8 W/(m·K)
Electrical Resistivity1.25 Ω·mm²/m
Thermal Expansion (20–100 °C)12.5 × 10⁻⁶/K
Tensile Strength Rm≥ 760 MPa
Yield Strength Rp0.2≥ 380 MPa
Elongation A5≥ 35%

Element Content acc. to VdTÜV Werkstoffblatt 499

CSiMnPSCo CrFeMo
≤ 0.030 ≤ 0.40≤0.50≤ 0.010≤ 0.010≤ 1.021.0 – 23.0≤ 5.08.0 – 10.0
NiTiAlNb + Al 
Balance≤ 0.40≤ 0.40 3.2 – 3.8 

  • Sheets and Plates – hot/cold rolled, solution annealed 
  • Bars and Rods – forged or rolled, pickled 
  • Tubes and Pipes – seamless or welded 
  • Wire – drawn or rolled 
  • Fittings and Flanges 
  • Forged and Machined Components – per drawing or specification 

Would you like a quotation?