• Element distribution in lean duplex stainless steel welds,  E.M. Westin, S. Hertzman, in press Welding in the World, 24pp.
  • IIW Doc. II-1807-12Effect of nitrogen-containing shielding and backing gas on the pitting corrosion resistance of welded lean duplex stainless steelLDX 2101® (EN 1.4162, UNS S32101), E.M. Westin, M.M. Johansson, R.F.A. Pettersson, accepted for publication in Welding in the World 57 (2013).
  • Welding stainless steels – Experience with water heaters , E.M. Westin, D. Serrander,  Welding in the World 56 (2012) 5/6 14pp.
  • Localized corrosion resistance of welded austenitic and lean duplex stainless steels, M.M. Johansson, E.M. Westin, J. Oliver, R.F.A. Pettersson, Welding in the World 55 (2011) 9/10 19-27.
  • Single-pass laser GMA hybrid welding of 13.5 mm thick duplex stainless steel, E.M. Westin, K. Stelling, A. Gumenyuk, Welding in the World, 55 (2011) 1/2 39-49.
  • Pitting corrosion resistance of GTA welded lean duplex stainless steel E.M. Westin, Welding in the World 54 (2010) 11/12 R308-321.
  • Effect of laser and laser hybrid welding on the corrosion performance of a lean duplex stainless steel, E.M. Westin, A. Fellman, Journal of Laser Applications, 22 (2010) 4 150-158.
  • Fracture toughness of welded commercial duplex stainless steel H. Sieurin, E.M. Westin, M. Liljas, R. Sandström, Welding in the World, 53 (2009) R24-R33.
  • Weld oxide formation on lean duplex stainless steel, E.M. Westin, C.-O.A. Olsson, S. Hertzman, Corrosion Science 50 (2008) 2620-2634.
  • Weldability aspects of a newly developed duplex stainless steel LDX 2101, E.M. Westin, B. Brolund, S. Hertzman, Steel Research International 79 (2008) 473-481.
  • Effect of post-weld straining on temper rolled austenitic stainless steel welds, H. Engström, E.M. Westin, Welding in the World 52 (2008) 1/2 87-99
  • Fracture toughness of the lean duplex stainless steel LDX 2101, H. Sieurin, R. Sandström, E.M. Westin, Metallurgical and Materials Transactions A, 37A (2006) 2975-2982.
  • Welding the lean duplex steel, LDX  2101® for pressure vessel applications down to -40°C design temperature, using a positional flux cored wire , F. Hägg, H. Åström
  • Welding of the new duplex grade LDX 2404® with 2209-type filler , L. Å. Bylund,  M. Johansson, R. Pettersson
  • Schweißen hochkorrosionsbeständiger Stähle; H. Heuser; Dechema Frankfurt, Januar 2005
  • Anforderungen an Schweißzusatzwerkstoffe hinsichtlich der Korrosionssicherheit; H. Heuser; Dechema Frankfurt, März 2004
  • Value of different hot cracking tests for the manufacture of filler metals; H. Heuser; BAM Berlin, März 2004